Skip to content
custom fiberglass manufacturers, fiberglass products manufacturers plastic insert molding

Managing Sink in Injection Molding Designs

Om Raj Tech
Om Raj Tech

Few defects frustrate product designers as much as sink marks. A part may be strong, accurate and functional, yet a small dimple on a visible surface can make it look cheap or flawed. Sink is one of the most common cosmetic and dimensional defects in plastic injection molding, but it is also one of the most preventable. With the right design, tooling and process choices, sink can be minimized or eliminated.

This guide explains what sink is, why it happens, and how to manage it through design, material, tooling and process decisions.

What are sink marks?

A sink mark is a small depression or dimple that forms on the surface of a molded part, typically opposite a thick feature such as a rib, boss or heavy wall. When molten plastic cools, it shrinks. The outer skin freezes first against the cold mold wall and becomes rigid, while the thicker interior stays hot and molten longer. As the core cools and contracts, it pulls the still-flexible surface inward, creating a visible depression. In severe cases, the core may even pull away from itself and form an internal void.

Why sink matters

Sink is more than a cosmetic problem. On appearance parts such as consumer products, automotive trim and visible housings, it can lead to rejects and customer complaints. On functional parts, sink can distort sealing surfaces, affect assembly fit and create stress concentrations. Fixing sink after tooling is built is expensive, so it is smart to address it during design.

Main causes of sink

  • Excessive thickness. Thick sections shrink more and cool more slowly, so they are the primary cause.
  • Rib and boss design. Ribs that are too thick or bosses that are too massive create hot spots behind visible surfaces.
  • Insufficient packing. Low packing pressure or short hold time fails to compensate for shrinkage.
  • Gate problems. Small or poorly placed gates freeze before the cavity is packed.
  • Cooling issues. Uneven or insufficient cooling leaves hot areas that shrink after the surface is set.
  • High melt or mold temperature. Hotter material shrinks more.
  • Material choice. Semi-crystalline resins with high shrinkage, such as polypropylene and nylon, are more prone to sink than amorphous ones.

Design solutions

Design is the most powerful and least expensive place to control sink.

  1. Keep wall thickness uniform. Aim for consistent walls throughout the part, and make transitions gradual rather than abrupt.
  2. Size ribs correctly. As a general rule, ribs should be about 50 to 60 percent of the adjoining wall thickness, or 40 percent for highly cosmetic surfaces with high-shrink materials.
  3. Design bosses carefully. Keep boss walls thin, connect them to the main wall with ribs and avoid placing heavy bosses directly behind visible areas.
  4. Core out thick sections. Hollow out heavy areas to reduce mass and maintain even wall thickness.
  5. Use radii. Generous fillets at intersections reduce hot spots and stress.
  6. Add surface features. Texture, grain, ribs, beads or intentional design lines can hide minor sink.
  7. Avoid thick sections near gates. If thickness is unavoidable, place the gate in the thick area so the material can be packed.

Material and shrinkage

Shrinkage varies by resin. Amorphous materials such as ABS and polycarbonate typically shrink between 0.4 and 0.8 percent, while semi-crystalline materials such as polypropylene and nylon can shrink from 1 to 2 percent or more. Fillers such as glass fiber lower shrinkage and reduce sink risk. If sink is a concern, consider reinforced grades or lower-shrink alternatives.

Tooling solutions

The mold can do a great deal to control sink.

  • Larger gates and shorter flow paths keep the gate open long enough to pack the part.
  • Gate location near thick features improves packing efficiency.
  • Balanced cooling channels remove heat evenly, especially behind ribs and bosses. Conformal cooling or beryllium-copper inserts can address hard-to-cool areas.
  • Venting prevents trapped air that can interfere with packing.
  • Texture on the cavity surface masks shallow sink effectively.

Our tooling specialists review gating, cooling and venting early so molds are built to minimize sink from the first shot.

Process solutions

Even a well-designed part depends on proper processing.

  • Increase packing pressure and hold time so more material is added as the part shrinks.
  • Lower melt temperature slightly to reduce overall shrinkage, within the material's recommended range.
  • Adjust mold temperature to balance skin formation and cooling time.
  • Extend cooling time so the core solidifies before ejection.
  • Optimize injection speed to improve packing and reduce stress.
  • Verify gate freeze-off time with a gate seal study to confirm that packing is effective.

Advanced techniques

When traditional methods are not enough, advanced processes can help. Gas-assist molding injects nitrogen into thick sections to hollow them and apply internal pressure. Foam molding uses a blowing agent to create internal pressure that offsets shrinkage. Variable mold temperature technology, also called rapid heat and cool, improves surface quality and packing. These methods add cost but can solve challenging sink problems on large or thick parts.

Using simulation

Mold-flow simulation predicts where sink and voids are likely to occur before any steel is cut. By testing different wall thicknesses, gate locations and cooling layouts virtually, designers can correct problems at the lowest-cost stage. Simulation also helps determine realistic packing and cooling parameters for production.

Troubleshooting checklist

  1. Confirm that the sink is located opposite a thick feature.
  2. Check packing pressure and hold time.
  3. Verify that the gate is not freezing prematurely.
  4. Review cooling efficiency around the affected area.
  5. Check melt and mold temperatures.
  6. Evaluate whether a design change, such as thinner ribs or coring, is possible.
  7. Consider a material with lower shrinkage if the geometry cannot change.

Get it right early

The cheapest time to fix sink is during design review. Our plastic injection molding engineers evaluate geometry for manufacturability, and our tooling group builds molds with cooling and gating that reduce defects. Customers searching for injection molding companies in Michigan trust Om Raj Tech to catch these issues early and deliver attractive, accurate parts.

Send us your CAD model and we will provide a manufacturability review that identifies potential sink areas and suggests practical solutions.

Share this post